treatment modulus # Elastic modulus (in kPa) of latex tubes after various # autoclaving treatments. There are five treatments: # 1 control (no autoclaving) # 2 low temperature low time # 3 low temperature high time # 4 high temperature low time # 5 high temperatures high time # Temperatures are 121 and 135 C # Times are 10 and 20 minutes # data from Zeeshan Syedain 1 1117.5 1 1076.2 1 951.1 2 732.8 2 750.3 2 707.8 3 596.0 3 648.6 3 713.9 4 565.4 4 623.4 4 608.0 5 510.9 5 664.6 5 484.9